Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 45700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 315 MPa
45700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60
Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
Ball Indentation Hardness 315 MPa
45700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60
Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Ball Indentation Hardness 315 MPa
45700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60
Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Ball Indentation Hardness 315 MPa
45700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50
Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p..
Ball Indentation Hardness 315 MPa
45700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-6H black PA*-GF60
Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Ball Indentation Hardness 315 MPa
45700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60
Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac..
Ball Indentation Hardness 315 MPa
45700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60
Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
Ball Indentation Hardness 315 MPa
45700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-6H PA*-GF60
Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide...
Copyright © lookpolymers.com All Rights Reserved