Mechanical Properties Metric English Comments
Ball Indentation Hardness 325 MPa
47100 psi
H 961/30; ISO 2039/P1
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat..
Ball Indentation Hardness 325 MPa
47100 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50
Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:..
Ball Indentation Hardness 325 MPa
47100 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50
Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:..
Ball Indentation Hardness 325 MPa
47100 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45
Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a..
Ball Indentation Hardness 325 MPa
47100 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45
Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY ..