Mechanical Properties Metric English Comments
Ball Indentation Hardness 500 MPa
72500 psi
H 961/30; ISO 2039/P1
Hexion Bakelite™ PF 6506 Phenolic Formaldehyde Resin, Low Shrinkage, Resistant to High Temperatures, UL Listed &nbs
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant, UL listed molding compound 1.5 mm/V-..