Polymer Property : Ball Indentation Hardness = 7540 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 52.0 MPa
7540 psi
DIN 53456
Global PP-3375-RM Polypropylene Random Copolymer
Description-medium stiffness, low melting temperatures, very good for seal Applications-fabricsInformation provided by Global Polymers Corporation.
Ball Indentation Hardness 52.0 MPa
7540 psi
DIN 53456
Global PP-3370-RM Polypropylene Random Copolymer
Description-medium stiffness, low melting temperatures, very good for seal Applications-filmInformation provided by Global Polymers Corporation.
Ball Indentation Hardness 52.0 MPa
7540 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-G15 PTFE
Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 52.0 - 56.0 MPa
7540 - 8120 psi
ISO 2032-N961
Adamas Adalon® 113 PTFE, 23/2% Carbon/Graphite Filled
Information provided by Adamas, HPM
Ball Indentation Hardness 52.0 MPa
7540 psi
132 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 300 HI6 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 52.0 - 56.0 MPa
7540 - 8120 psi
ISO 2032-N961
Adamas Adalon® 131 PTFE, 25% Soft Carbon Filled
Information provided by Adamas, HPM
Ball Indentation Hardness 52.0 MPa
7540 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-B60 PTFE
Tarflen SM1 reinforced with 60% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.