Polymer Property : Ball Indentation Hardness = 7980 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 50.0 - 55.0 MPa
7250 - 7980 psi
ISO 2032-N132
Adamas Adalon® 237 PTFE, 25% Glass Fiber
Information provided by Adamas, HPM
Ball Indentation Hardness 50.0 - 55.0 MPa
7250 - 7980 psi
ISO 2032-N132
Adamas Adalon® 252 PTFE, 28% Glass Fiber
Information provided by Adamas, HPM
Ball Indentation Hardness 50.0 - 55.0 MPa
7250 - 7980 psi
ISO 2032-N132
Adamas Adalon® 406 PTFE, 15% PEEK
Information provided by Adamas, HPM
Ball Indentation Hardness 50.0 - 55.0 MPa
7250 - 7980 psi
ISO 2032
Adamas Adalon® 509 PTFE, 3% MoS2
Information provided by Adamas, HPM