Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 88.5 MPa | 12800 psi | 358 N/30s; ISO 2039 |
Borealis ME212U Polypropylene Compound, Mineral Filled ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air.. |