Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.172 MPa @Strain 3.00 % |
25.0 psi @Strain 3.00 % |
Load applied parallel to fiber plane |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Compressive Yield Strength | 0.172 MPa @Strain 40.0 % |
24.9 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD50CN Conductive Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |