Mechanical Properties Metric English Comments
Compressive Yield Strength 0.184 MPa

@Strain 50.0 %
26.7 psi

@Strain 50.0 %
BS ISO 7214 1998
Zotefoams Evazote® EV70CN Conductive Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Compressive Yield Strength 0.184 MPa

@Strain 50.0 %
26.7 psi

@Strain 50.0 %
BS ISO 7214 1998
Zotefoams Evazote® VA80 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Compressive Yield Strength 0.184 MPa

@Strain 40.0 %
26.7 psi

@Strain 40.0 %
BS ISO 7214 1998
Zotefoams Plastazote® HD30 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..