Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 103.1 MPa @Strain 10.0 % |
14950 psi @Strain 10.0 % |
ASTM D695 |
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe.. |