Polymer Property : Compressive Yield Strength = 103000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 710 MPa

@Temperature 104 °C
103000 psi

@Temperature 220 °F
0°, Dry, Fill Compression
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber
Information provided by HexCel
Compressive Yield Strength 710 MPa

@Temperature 23.0 °C
103000 psi

@Temperature 73.4 °F
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement
Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% VoidsInformation provided by HexCel