Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 75.0 MPa @Strain 5.00 % |
10900 psi @Strain 5.00 % |
dry; ISO 604 |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Compressive Yield Strength | 75.0 MPa @Strain 2.00 % |
10900 psi @Strain 2.00 % |
dry; ISO 604 |
Murtfeldt Murpec® Polyetheretherketone In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change.. |