Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1117 MPa @Temperature 24.0 °C |
162000 psi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, T2C145 Carbon Tape Hexcel designation: T_145-12"-F522; Various Fibers; (145 g/m2)Information provided by HexCel |