Polymer Property : Compressive Yield Strength = 124 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 124 MPa

@Strain 10.0 %
18000 psi

@Strain 10.0 %
ASTM D695
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide
Melidin® 7021 CM is a self-lubricating compression molded polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best fo..