Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 133 MPa @Strain 10.0 % |
19300 psi @Strain 10.0 % |
ASTM D695 |
Saint-Gobain Meldin® 7021 Isostatically Molded Graphite Filled Polyimide Melidin® 7021 is a self-lubricating thermosetting polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best for high t.. |