Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 116 MPa @Strain 1.00 % |
16800 psi @Strain 1.00 % |
1% offset; ASTM D695 |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |