Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 117 MPa @Strain 10.0 % |
17000 psi @Strain 10.0 % |
ASTM D695 |
Saint-Gobain Meldin® 7003 CM Compression Molded MoS2 Filled Polyimide Melidin® 7003 CM is a compression molded polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions.Specific.. |
|||
Compressive Yield Strength | 117 MPa @Temperature 71.0 °C |
17000 psi @Temperature 160 °F |
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C) |
Hexcel® HexPly® F522 Epoxy Resin, K285 Kevlar® Fabric Hexcel designation: K285-38"-F522; Kev. 49 1140Information provided by HexCel |
|||
Compressive Yield Strength | 117 MPa @Temperature 132 °C |
17000 psi @Temperature 270 °F |
Dry |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |
|||
Compressive Yield Strength | 117 MPa @Strain 10.0 %, Temperature 23.0 °C |
17000 psi @Strain 10.0 %, Temperature 73.4 °F |
ASTM D695 Modified |
Saint-Gobain Meldin® 2030 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |