Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1185 MPa @Temperature 71.0 °C |
171900 psi @Temperature 160 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, T3T190 Carbon Tape Hexcel designation: T_190-12"-F263; Various fibersInformation provided by HexCel |