Compressive Yield Strength 128 MPa

@Strain 10.0 %
18500 psi

@Strain 10.0 %
ASTM D695
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide
Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide ..