Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 181 MPa @Temperature 23.0 °C |
26300 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form Fiber: IM7-12KInformation provided by HexCel |