Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 31.0 MPa @Temperature 22.0 °C |
4500 psi @Temperature 71.6 °F |
Block Compression; Cure Cycle: 60 min @ 120°C/248°F; ASTM D695 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |