Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 228 MPa @Temperature 25.0 °C |
33100 psi @Temperature 77.0 °F |
After 3000 in-inlb/in impact |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |