Compressive Yield Strength 0.0330 MPa

@Strain 10.0 %
4.79 psi

@Strain 10.0 %
BS ISO 7214 1998
Zotefoams Plastazote® LD18 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Compressive Yield Strength 0.0330 MPa

@Strain 10.0 %
4.79 psi

@Strain 10.0 %
BS ISO 7214 1998
Zotefoams Plastazote® LD24MC Low Density Polyethylene Foam, Medium Cell