Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 400 MPa @Temperature 71.0 °C |
58000 psi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 181 Glass Fabric Information provided by HexCel |
|||
Compressive Yield Strength | 400 MPa @Temperature 71.0 °C |
58000 psi @Temperature 160 °F |
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C) |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |