Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 526 MPa @Temperature 25.0 °C |
76300 psi @Temperature 77.0 °F |
Compression Before Impact, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A280-5H Fiber Information provided by HexCel |