Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 408 MPa @Temperature 177 °C |
59200 psi @Temperature 351 °F |
AS4C; Fill Compression; Wet condition |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |