Polymer Property : Compressive Yield Strength = 77.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 77.2 MPa

@Strain 10.0 %
11200 psi

@Strain 10.0 %
ASTM D695
Saint-Gobain Meldin® 7211 DF Direct Formed Graphite and PTFE Filled Polyimide
Melidin® 7211 DF is a direct formed polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Specific..