Polymer Property : Compressive Yield Strength = 77000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 531 MPa

@Temperature 232 °C
77000 psi

@Temperature 450 °F
AS4C; Fill Compression;
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel