Polymer Property : Compressive Yield Strength = 79.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 79.0 MPa

@Strain 5.00 %
11500 psi

@Strain 5.00 %
dry; ISO 604
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..
Compressive Yield Strength 79.0 MPa

@Strain 5.00 %
11500 psi

@Strain 5.00 %
dry; ISO 604
Murtfeldt Murlubric® Oil Modified Nylon 6
Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi..