Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0207 - 0.0552 MPa @Strain 25.0 % |
3.00 - 8.00 psi @Strain 25.0 % |
Range, 0.2"/min. strain rate |
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena.. |
|||
Compressive Yield Strength | 0.0207 - 0.0552 MPa @Strain 25.0 % |
3.00 - 8.00 psi @Strain 25.0 % |
Range, 0.2"/min. strain rate |
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement. Standard available thickness 0.064"Features and Benefits of PORON Products: Excelle.. |