Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 86.0 MPa @Strain 2.00 % |
12500 psi @Strain 2.00 % |
dry; ISO 604 |
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |