Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 90.0 MPa

@Strain 5.00 %
13100 psi

@Strain 5.00 %
dry; ISO 604
Murtfeldt Murylon® A GF Nylon 66, Glass Reinforced
Murylon® A’s impressive characteristics are enhanced with admixed glass fibers. This results in a clear improvement in cold flow behavior and dimensional stability, enabling higher static pressure..
Compressive Yield Strength 90.0 MPa

@Temperature 177 °C
13100 psi

@Temperature 351 °F
Dry
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel