Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 917 MPa @Temperature 177 °C |
133000 psi @Temperature 351 °F |
[0°]; Resin Content=29%, Fiber Volume=64%; Wet condition-96 hours in boiling H2O |
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel |