Polymer Property : Compressive Yield Strength = 96.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 96.5 MPa

@Strain 10.0 %
14000 psi

@Strain 10.0 %
ASTM D695
Saint-Gobain Meldin® 7022 DF Direct Formed Graphite Filled Polyimide
Melidin® 7022 DF is a direct formed polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin® ..