Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 W-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | DIN 53453 |
Nilit FRIANYL C73 H-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
Radici Radilon® CS38FL (dry) Copolyamide 6 semiaromatic Film gradeInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 |
Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® A1S25 G15 PA66 15% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® PSB 286 PA6, DRY Description: Unreinforced polyamide PA6, with very good lubrication, standard for fast injection cycles, for injection molding.Available in: North AmericaProduct Applications: This grade has high fl.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EF040AE TPO Compound Daplen EF040AE is a elastomer modified polypropylene compound intended for injection molding. Daplen EF040AE is a material with excellent impact/stiffness ratio. Thanks to its low thermal expansio.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 9760 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9760 is heterophasic copolymer. PPC 9760 is characterized by improved stiffness, creep resistance and high impact resistance. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT) 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on pol.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 500 UV POM High flow injection molding grade based on Tarnoform 500 modified with carbon black giving best weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® B3K PA6 (Dry) Ultramid B 3K is an easy flowing, stabilized for fast processing, grade of nylon 6. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/IeA |
Addiplast Addinyl C2 V15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 GF25 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |