Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.254 J/cm² | 1.21 ft-lb/in² | ASTM D256 |
Plenco 1501 Polyester, Briquette, Transfer Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Charpy Impact, Notched | 0.254 J/cm² | 1.21 ft-lb/in² | ASTM D256 |
Plenco 7203 Phenolic, Granular, Transfer Molded PLENCO 07203 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and an industrial finish. UL recognized under component file E40654. 07203 is available i.. |