Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.504 J/cm² @Temperature 22.8 °C |
2.40 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ CMW 402 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive under-the-hood applications. Availability: Africa & Middle East, Asia Pacific, Europe, South America and North.. |