Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.120 - 0.180 J/cm² @Temperature 23.0 °C |
0.571 - 0.857 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/1eA |
Raschig Group 6501 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |