Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.300 - 1.05 J/cm² | 1.43 - 5.00 ft-lb/in² | Average value: 0.651 J/cm² Grade Count:55 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact, Notched | 0.340 - 1.05 J/cm² @Temperature -30.0 - -30.0 °C |
1.62 - 5.00 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.707 J/cm² Grade Count:8 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |