Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.271 J/cm²
1.29 ft-lb/in²
ASTM D256
Plenco 1530 Polyester, Briquette, Injection Molded
PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab..