Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.325 J/cm² | 1.55 ft-lb/in² | ISO 179-1:2007 |
CRP Technology Windform® FX Polyamide Composite Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive.. |