Charpy Impact, Notched 1.83 J/cm²
8.71 ft-lb/in²
Eastman Tenite 180A-28(HT) Cellulose Acetate  (discontinued **)
28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical.