Polymer Property : Charpy Impact, Notched = 1.85 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.85 J/cm²
8.80 ft-lb/in²
ISO 179/1EA-1993
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50
Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an..
Charpy Impact, Notched 1.85 J/cm²
8.80 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Charpy Impact, Notched 1.85 J/cm²
8.80 ft-lb/in²
ISO 179/1eA
Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..