Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.150 - 2.40 J/cm²
0.714 - 11.4 ft-lb/in²
Average value: 1.20 J/cm² Grade Count:40
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Charpy Impact, Notched 0.300 - 2.40 J/cm²
1.43 - 11.4 ft-lb/in²
Average value: 0.904 J/cm² Grade Count:112
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..