Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.17 J/cm²
10.3 ft-lb/in²
Eastman Tenite 371A-12 CAP Cellulose Acetate Propionate  (discontinued **)
12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 2.17 J/cm²
10.3 ft-lb/in²
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned)
Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas..