Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.42 J/cm²

@Temperature -30.0 °C
11.5 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® MB 3945 Nylon 11, Rotomolding Grade (Conditioned)
Designation ISO 1874-PA11-P,RDR,12-004Semi-rigid grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyeth..