Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.100 - 2.90 J/cm² @Temperature -40.0 - -20.0 °C |
0.476 - 13.8 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.28 J/cm² Grade Count:69 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |