Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
ISO 179/1eA
Radici Radilon® SHS (dry) Nylon 6
General PurposeInformation provided by Radici group.
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
EN ISO 179/1eA
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex
Charpy Impact, Notched 0.620 J/cm²

@Temperature -30.0 °C
2.95 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastar DN004 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Crastin® CE15315 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0..
Charpy Impact, Notched 0.620 J/cm²

@Temperature -30.0 °C
2.95 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Crastin® CE15315 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0..
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m..
Charpy Impact, Notched 0.620 J/cm²

@Temperature -30.0 °C
2.95 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® PLS FR95G15DH2 BK269 Nylon 6
15% Glass Reinforced Flame Retardant Heat Stabilized Polyamide Zytel PLSFR95G15DH2 BK269 is 15% glass reinforced flame retardant black PA using SHIELD Technology only from DuPont exceptional resista..
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
ISO R179
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6
Information provided by Arkema Group
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
1eA; ISO 179
Azoty Tarnow™ TARNOFORM 300 SI POM
Tribological modified grade with silicon, for better sliding properties in plastic-plastic contact.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Charpy Impact, Notched 0.620 J/cm²
2.95 ft-lb/in²
ASTM D256
Plenco 7552 Phenolic, Nodular, Transfer Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..
Charpy Impact, Notched 0.620 - 1.15 J/cm²
2.95 - 5.47 ft-lb/in²
Average value: 0.919 J/cm² Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant