Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.500 - 4.30 J/cm²
2.38 - 20.5 ft-lb/in²
Average value: 1.99 J/cm² Grade Count:34
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..