Polymer Property : Charpy Impact, Notched = 20.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 4.40 J/cm²
20.9 ft-lb/in²
DIN 53453
Nilit FRIANYL A63 HS28 Nylon 6.6 for injection molding
Nylon 6.6 for injection molding, maximum cold and dry impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS
Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance.
Charpy Impact, Notched 4.40 J/cm²
20.9 ft-lb/in²
ISO Data
Styron Magnumâ„¢ HPC 952 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..