Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.480 - 0.640 J/cm²

@Temperature -30.0 - -30.0 °C
2.28 - 3.05 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.575 J/cm² Grade Count:6
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..